Abstract
A novel selective sorption material allowing 99% Eu(III) recovery from Csl solutions was obtained by non-covalent immobilization of 5,11,17,23-tetrakis(diisoprpoxyphosphorylmethyl)25,26,27,28- tetrahydroxythiacalix[4]arene on silanized silica gel surface. According to the elemental analysis, the material contains 10 wt.% of thiacalixarene; specific surface area of the material under study is ~300 m2/g. The maximum recovery rate of Eu(III) ions is achieved within the pH range of 5.5–6.5 with the contact time of 24 h and is practically independent of CsI concentration in solution. The Eu(III) ions distribution coefficient reached 14.6 L/g. It was found that quantitative desorption of Eu(III) ions from the sorbent surface was ensured by using 1.5 M HNO3 solution as an eluent. The sorption preconcentration procedure followed by ICP-OES determination of Eu(III) in CsI single crystals and CsI raw material within the Eu(III) concentration range of 5∙10-7-1∙10-5 wt.% with the relative standard deviation as low as 5% was developed.
How to cite
M.S. Lukashova, S.G. Kharchenko, K.N. Belikov, E.Yu. Bryleva, N.N. Grebenyuk, I. B. Shcherbakov, V.I. Kalchenko. Sorption Preconcentration of Eu(III) Ions from CsI Solutions by Silica Gel Impregnated with 5,11,17,23-tetrakis(diisopropoxyphosphorylmethyl) 25,26,27,28-tetrahydroxythiacalix[4]arene. Methods Objects Chem. Anal. 2015, 10(3), 143-149. https://doi.org/10.17721/moca.2015.143-149